Chemical Composition of P265GH Steel
|
EN 10028-2
|
С
|
<0,2
|
Si
|
<0,4
|
Mn
|
0.6-1.4
|
P
|
<0,025
|
S
|
<0.01
|
Cr
|
<0,3
|
Mo
|
<0.08
|
Ni
|
<0,3
|
V
|
<0.02
|
Nb
|
<0.02
|
Ti
|
<0.03
|
Al
|
>0.02
|
Cu
|
<0,3
|
N
|
<0.012
|
Fe
|
Other
|
Mechanical properties of P265GH material
Per EN 10028-2
|
|
+N
|
|
Nominal thickness, (mm)
|
< 16
|
16 – 40
|
40 – 60
|
60 – 100
|
100 – 150
|
150 – 200
|
|
Minimum yield strength, ReH (MPa)
|
265
|
255
|
245
|
215
|
200
|
185
|
|
Tensile strength (tensile strength) , Rm (MPa)
|
410-530
|
410-530
|
410-530
|
410-530
|
400-530
|
390-530
|
|
Minimum elongation after break, A (%)
|
22
|
|
|
Minimum absorbed energy at 20°C, J (J )
|
40
|
|
|
Minimum absorbed energy at 0°C 32°F], J (J)
|
34
|
|
Minimum absorbed energy at -20°C, J (J)
|
27
|
|
Yield strength at 50°C, ReH (MPa)
|
256
|
247
|
237
|
208
|
193
|
179
|
|
Yield strength at 100°C, ReH (MPa)
|
241
|
232
|
223
|
196
|
182
|
168
|
|
Yield strength at 150°C, ReH (MPa)
|
223
|
215
|
206
|
181
|
169
|
156
|
|
Yield strength at 200°C, ReH (MPa)
|
205
|
197
|
190
|
167
|
155
|
143
|
|
Yield strength at 250°C, ReH (MPa)
|
188
|
181
|
174
|
153
|
142
|
131
|
|
Yield strength at 300°C, ReH (MPa)
|
173
|
166
|
160
|
140
|
130
|
121
|
|
Yield strength at 350°C, ReH (MPa)
|
160
|
154
|
148
|
130
|
121
|
112
|
|
Yield strength at 400°C, ReH (MPa)
|
150
|
145
|
139
|
122
|
114
|
105
|
|